Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.60 µm/m-°C @Temperature 20.0 - 300 °C |
3.67 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
Schott Glass 8326 Neutral Glass Tubing Neutral glass tubing, alkali resistance better as for DURAN® Special lab glass The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is less than 100 ppm.Info.. |
|||
CTE, linear | 6.60 µm/m-°C @Temperature 20.0 - 300 °C |
3.67 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
Schott Glass 8436 Particularly resistant to sodium vapor and alkaline solutions, suitable to combinations with sapphire glass.Information provided by SCHOTT AG. |
|||
CTE, linear | 6.61 µm/m-°C @Temperature 20.0 - 400 °C |
3.67 µin/in-°F @Temperature 68.0 - 752 °F |
|
ATI Wah Chang Infiltrated Tungsten (Copper) Tungsten base infiltrated metal with Copper as infiltrant has been widely used in industry for years. It has proven highly advantageous because of its excellent machinability. Roughly 90% Tungsten a.. |