Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.10 µm/m-°C @Temperature 20.0 °C |
3.39 µin/in-°F @Temperature 68.0 °F |
|
Pyrotek Valcor® G-AZ Pre-Cast Shapes ApplicationsBurner blocks Skimmer blocks Cover blocks Specialty blocks Plungers Stirrers Spouts Feeder tubes AdvantagesProven performance in molten glass contact applications Smooth surface finish d.. |
|||
CTE, linear | 6.10 µm/m-°C | 3.39 µin/in-°F | at Set Pt. (Fired Thermal Expansion) |
Ferro CF 7578 Low-Temperature Sealing DEVITRIFYING Typical Powder Form: VSD Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific .. |
|||
CTE, linear | 6.10 µm/m-°C @Temperature 20.0 °C |
3.39 µin/in-°F @Temperature 68.0 °F |
|
CMW® THERMKON® 62 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
CTE, linear | 6.10 µm/m-°C @Temperature 20.0 - 1093 °C |
3.39 µin/in-°F @Temperature 68.0 - 1999 °F |
|
BNZ Materials BNZ-28 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
CTE, linear | 6.10 µm/m-°C @Temperature 20.0 - 1093 °C |
3.39 µin/in-°F @Temperature 68.0 - 1999 °F |
|
BNZ Materials BNZ-3000 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
CTE, linear | 6.10 µm/m-°C @Temperature 20.0 - 1093 °C |
3.39 µin/in-°F @Temperature 68.0 - 1999 °F |
|
BNZ Materials BNZ-32 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
CTE, linear | 6.10 µm/m-°C @Temperature 27.0 - 175 °C |
3.39 µin/in-°F @Temperature 80.6 - 347 °F |
ASTM D696 |
3M 7945MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
CTE, linear | 6.10 µm/m-°C @Temperature 27.0 - 175 °C |
3.39 µin/in-°F @Temperature 80.6 - 347 °F |
ASTM D696 |
3M 9045MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |