Thermal Properties Metric English Comments
CTE, linear 5.90 µm/m-°C

@Temperature 50.0 - 500 °C
3.28 µin/in-°F

@Temperature 122 - 932 °F
Pre-fired 1200°C
Old Hickory No. 1 Glaze Kentucky Ball Clay
No. 1 Glaze Clay is a very high kaolin bearing selection with extremely low levels of carbon content. it provides excellent suspension to all types of glazes especially glazes containing a high perc..
CTE, linear 5.90 µm/m-°C

@Temperature 20.0 - 1000 °C
3.28 µin/in-°F

@Temperature 68.0 - 1830 °F
McDanel Advanced Ceramics MV-HR1 Mullite
Mullite (3Al2O3 • 2SiO2) is a refractory oxide material combining low thermal expansion, good mechanical strength, and resilience at elevated temperatures. Mullite is formulated to produce den..