Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 38.0 µm/m-°C @Temperature 20.0 °C |
21.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Resinoid 7051 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
CTE, linear | 38.0 µm/m-°C @Temperature 20.0 °C |
21.1 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
Teijin Multilon DN-1520B Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has improved stiffness through the addition of 20 % filler. Improved stiffness and high fluidity realizes a thin wall.. |
|||
CTE, linear | 38.0 µm/m-°C | 21.1 µin/in-°F | via TMA |
Specialty Coating Systems Parylene D Poly (P-Xylylene) Coating Parylene D is a polymer of para-xylylene modified by the substitution of chlorine atoms for two of the aromatic hydrogen atoms. Parylene D is similar in properties to Parylene C with the added abili.. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
21.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL GTX CRN720V PPE+PA6 (Asia Pacific) GF20% FR-GTX, Restricted to sell for new customers |
|||
CTE, linear | 38.0 µm/m-°C @Temperature 40.0 - 130 °C |
21.1 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 05118-T5 Phenolic, Granular, Compression Molded PLENCO 05118-T5 is a mineral and graphite filled novolac phenolic molding compound with PTFE, formulated for bearing seals. 05118 provides for a low coefficient of friction, good wear resistance, ve.. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature 40.0 - 130 °C |
21.1 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 4349 Phenolic, Granular, Transfer Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature 20.0 °C |
21.1 µin/in-°F @Temperature 68.0 °F |
|
Williams Advanced Alloys WS96 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
CTE, linear | 38.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
21.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
D696 |
Zhejiang Juner 301-G15 15% Glass Fibre Reinforced and Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature 20.0 °C |
21.1 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Bond 2123 Metal Repair Steel/Epoxy Adhesive TRA-BOND 2123 is a versatile steel metal/epoxy adhesive formulation developed for modern industrial repair, casting and bonding applications where a steel-like or cast iron finish is required. This .. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature 50.0 - 200 °C |
21.1 µin/in-°F @Temperature 122 - 392 °F |
DIN 53 752 |
Ensinger TECASINT 1021 Polyimide, 15% Graphite Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
CTE, linear | 38.0 µm/m-°C | 21.1 µin/in-°F | ASTM D696 |
Ensinger TECATOR™ GF30 (XP142T) Polyamide-imide (PAI), 30% glass filled, compression molded TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger .. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature 20.0 °C |
21.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Devcon Magic Bond™ Epoxy Putty Emergency Repair ProductsComments: Two-part epoxy putty stick seals leaks and repairs gouges in steel, aluminum, wood, fiberglass, concrete and ceramics. Cures rock-hard and can be painted, sanded,.. |
|||
CTE, linear | 38.0 µm/m-°C | 21.1 µin/in-°F | Below Tg |
Epoxy Technology EPO-TEK® EK1000 Epoxy Material Description: A single component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance making it ideal for the demanding .. |
|||
CTE, linear | 38.0 µm/m-°C | 21.1 µin/in-°F | Below Tg |
Epoxy Technology EPO-TEK® EK1000-MP Epoxy Material Description: A single component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance making it ideal for the demanding .. |
|||
CTE, linear | 38.0 µm/m-°C | 21.1 µin/in-°F | Below Tg |
Epoxy Technology EPO-TEK® EK2000 Epoxy Preliminary Product Information SheetMaterial Description: A two component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance .. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
21.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry) Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also.. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
21.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Dry) Ultramid 8233G HS BK-102 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature performance and d.. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
21.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM Test |
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Dry) Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature
performance and .. |
|||
CTE, linear | 38.0 µm/m-°C | 21.1 µin/in-°F | ASTM E831 |
BASF Ultramid® HPN 9233G HS BK 102 33% Glass Filled PA6 (Dry) Description: Ultramid HPN 9233G HS BK-102 is a heat stabilized, pigmented black, 33% glass reinforced PA6 injection molding grade resin in the High Productivity Nylon Series developed for improved c.. |
|||
CTE, linear | 38.0 µm/m-°C | 21.1 µin/in-°F | |
Atom Adhesives AA-BOND 2123 Epoxy Adhesive AA-BOND 2123 is a versatile steel metal/epoxy adhesive formulation developed for modern industrial repair, casting and bonding applications where a steel-like or cast iron finish is required. AA-BON.. |
|||
CTE, linear | 38.0 - 42.0 µm/m-°C @Temperature 20.0 - 125 °C |
21.1 - 23.3 µin/in-°F @Temperature 68.0 - 257 °F |
|
Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a.. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
21.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
Beijing Chemical Industry KAIFA® 301-G15 PBT Resin 15% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
CTE, linear | 38.0 - 42.0 µm/m-°C @Temperature 20.0 - 125 °C |
21.1 - 23.3 µin/in-°F @Temperature 68.0 - 257 °F |
|
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar.. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature 20.0 °C |
21.1 µin/in-°F @Temperature 68.0 °F |
ASTM data |
BASF Capron® HPN 9233G HS BK-102 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron HPN 9233G HS BK-102 is a heat stabilized, pigmented black, 33% glass reinforced nylon 6 injection molding grade resin in the High Productivity Nylon Series developed for improved cycle times .. |
|||
CTE, linear | 38.0 µm/m-°C @Temperature 20.0 °C |
21.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Resinoid 7051 SS Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |