Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.80 µm/m-°C @Temperature 260 °C |
2.67 µin/in-°F @Temperature 500 °F |
Fired Thermal Expansion |
Ferro EG 2000 Low-Temperature Sealing VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp.. |
|||
CTE, linear | 4.80 µm/m-°C @Temperature 25.0 - 260 °C |
2.67 µin/in-°F @Temperature 77.0 - 500 °F |
|
Ferro IP 760 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
CTE, linear | 4.80 µm/m-°C | 2.67 µin/in-°F | at Set Pt. |
Ferro IX 2218 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: REG, MVG Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a.. |
|||
CTE, linear | 4.80 µm/m-°C @Temperature 260 °C |
2.67 µin/in-°F @Temperature 500 °F |
|
Ferro IX 2218 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: REG, MVG Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a.. |
|||
CTE, linear | 4.80 µm/m-°C @Temperature 25.0 - 260 °C |
2.67 µin/in-°F @Temperature 77.0 - 500 °F |
|
Ferro IP 745 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
CTE, linear | 4.80 µm/m-°C @Temperature 25.0 - 100 °C |
2.67 µin/in-°F @Temperature 77.0 - 212 °F |
ASTM E831 |
M Cubed Technologies RBBC-751 Reaction Bonded Boron Carbide Reaction-bonded boron carbide for extreme wear environments. Can be cast into very large components (greater than 4 ft. square)Information provided by M Cubed Technologies, Inc. |
|||
CTE, linear | 4.80 µm/m-°C @Temperature 1000 °C |
2.67 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SB65S Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.80 µm/m-°C @Temperature 1000 °C |
2.67 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SC80 Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 4.80 µm/m-°C | 2.67 µin/in-°F | Volumetric thermal expansion |
China-Yixing Longly Refractories ASM-130 Cordierite-Mullite Featured mullite, cordierite as the main raw material, the use of advanced production technology, professionally manufacturing the kiln furniture of ceramic and powder metallurgy with load bearing b.. |
|||
CTE, linear | 4.80 µm/m-°C | 2.67 µin/in-°F | |
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |
|||
CTE, linear | 4.80 µm/m-°C @Temperature 20.0 - 1000 °C |
2.67 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Ceradyne CeraTrex™ 146-3E Silicon Carbide Features:high puritycorrosion resistancewear resistancetailored electrical properties Applications:semiconductor componentssputtering targetsballistic armorwear componentsInformation provided by Cer.. |
|||
CTE, linear | 4.80 µm/m-°C @Temperature 20.0 - 1000 °C |
2.67 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Ceradyne CeraTrex™ 146-IS Silicon Carbide Features:high puritycorrosion resistancewear resistanceApplications:semiconductor componentssputtering targetsInformation provided by Ceradyne Company |