Thermal Properties Metric English Comments
CTE, linear 4.55 µm/m-°C

@Temperature 260 °C
2.53 µin/in-°F

@Temperature 500 °F
Ferro EG 0024 Specialty Glass
Glass Type: Si-B-MG-Al Typical Powder Form: VWG Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-ph..