Thermal Properties Metric English Comments
CTE, linear <= 4.30 µm/m-°C

@Temperature 20.0 °C
<= 2.39 µin/in-°F

@Temperature 68.0 °F
MarkeTech AN 120 Aluminum Nitride Ceramic Substrate, 98% Purity
Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 µ..
CTE, linear >= 4.30 µm/m-°C

@Temperature 20.0 °C
>= 2.39 µin/in-°F

@Temperature 68.0 °F
MarkeTech AN 160 Aluminum Nitride Ceramic Substrate, 99% Purity
Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 µ..
CTE, linear 4.30 µm/m-°C

@Temperature 20.0 - 1000 °C
2.39 µin/in-°F

@Temperature 68.0 - 1830 °F
ASTM C-372
Skamol Group SICAL 78 Silicon Nitride-Bonded Silicon Carbide Brick
Silicon nitride-bonded silicon carbide brick has the following characteristics: Max. service temperature 1580°C (2876°F)For sidewall lining of aluminum reduction cellsHigh thermal conductivity..
CTE, linear 4.30 µm/m-°C

@Temperature 20.0 °C
2.39 µin/in-°F

@Temperature 68.0 °F
Sapco Si.SiC Silicon Carbide
Information provided by Sapco.
CTE, linear 4.30 µm/m-°C
2.39 µin/in-°F
Tokuyama Shapal™ SH-15 Sintered Aluminum Nitride
Uniform, large sized pressed sintered aluminum nitride.
CTE, linear 4.30 µm/m-°C

@Temperature 25.0 - 1000 °C
2.39 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek Reaction Bonded Silicon Carbide, SCRB (SC-2)
Thermal Shock Delta Tc = 400°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
CTE, linear 4.30 µm/m-°C

@Temperature 1000 °C
2.39 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CRAG-S81 Long Stopper
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 4.30 µm/m-°C

@Temperature 1000 °C
2.39 µin/in-°F

@Temperature 1830 °F
Chosun Refractories SBSN Bricks, Reaction Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 4.30 µm/m-°C

@Temperature 1000 °C
2.39 µin/in-°F

@Temperature 1830 °F
Chosun Refractories SSB-3 Bricks, Reaction Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 4.30 µm/m-°C

@Temperature 20.0 - 1000 °C
2.39 µin/in-°F

@Temperature 68.0 - 1830 °F
Ceradyne Ceralloy® 1370CS AlN