Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 3.80 µm/m-°C @Temperature 21.1 - 449 °C |
2.11 µin/in-°F @Temperature 70.0 - 840 °F |
|
PSM Industries Ferro-TiC® PK Maraging Steel Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Comb.. |
|||
CTE, linear | 3.80 µm/m-°C | 2.11 µin/in-°F | at Set Pt. |
Ferro EG 0002 Glazes and Sealants Glass Type: Si-Al-Ba Typical Powder Form: VWG Typical Application: SiC Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insulatin.. |
|||
CTE, linear | 3.80 µm/m-°C | 2.11 µin/in-°F | at Set Pt. (Fired Thermal Expansion) |
Ferro EG 2805 Low-Temperature Sealing VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp.. |
|||
CTE, linear | 3.80 µm/m-°C @Temperature 20.0 - 300 °C |
2.11 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
Schott Glass 8448 Intermediate Sealing Glass Intermediate sealing glass Sealing to the glasses 8330, 8449, 8486, 8487, and tungstenInformation provided by SCHOTT AG. |
|||
CTE, linear | 3.80 µm/m-°C @Temperature 20.0 - 300 °C |
2.11 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
Schott Glass 8688 Borosilicate Glass Borosilicate glass, highly UV-blocked, stabilized against solarization, sealing glass to Tungsten Backlights The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium.. |
|||
CTE, linear | 3.80 µm/m-°C @Temperature 20.0 - 300 °C |
2.11 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
Schott Glass 8689 Borosilicate Glass Borosilicate glass, highly UV-blocked, stabilized against solarization, sealing glass to Tungsten Backlights The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium.. |
|||
CTE, linear | 3.80 µm/m-°C @Temperature 20.0 °C |
2.11 µin/in-°F @Temperature 68.0 °F |
|
Sapco S.SiC Silicon Carbide Information provided by Sapco. |