Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 335 µm/m-°C | 186 µin/in-°F | Silicone Property; ASTM E 831 |
Arlon R36798T017 0.017" (0.432 mm) Uncured Silicone Rubber with Laminated Tefzel® Substrate
(discontinue Design/Construction: Liner: PTFE Coated Fiberglass Side 1: Uncured Silicone Rubber Substrate: Laminated Tefzel® Substrate: Treated for adhesionAppearance: Translucent, high viscosity gum on fluoro.. |
|||
CTE, linear | 335 µm/m-°C @Temperature 20.0 °C |
186 µin/in-°F @Temperature 68.0 °F |
Silicone Property; ASTM E 831 |
Arlon 25188T010 Silicone Rubber/Laminated ETFE Film Liner: 3 mil PTFE coated fiberglass; Side 1: uncured silicone rubber; Substrate: laminated ETFE film, treated for adhesion |
|||
CTE, linear | 335 µm/m-°C @Temperature 20.0 °C |
186 µin/in-°F @Temperature 68.0 °F |
Silicone Property; ASTM E 831 |
Arlon 25188T017 Silicone Rubber/Laminated ETFE Film Liner: 3 mil PTFE coated fiberglass; Side 1: uncured silicone rubber; Substrate: laminated ETFE film, treated for adhesion |
|||
CTE, linear | 335 µm/m-°C | 186 µin/in-°F | Silicone Property; Arlon SQA-TMS-022 |
Arlon 25188T020 0.020" Uncured Silicone Rubber/Laminated ETFE Film Design/Construction:Liner: 0.003" PTFE Coated FiberglassSide 1: Uncured Silicone RubberSubstrate: Laminated ETFE Film-treated for adhesionThis data represents typical values for the production ma.. |
|||
CTE, linear | 335 µm/m-°C | 186 µin/in-°F | Silicone Property; ASTM E 831 |
Arlon R37208T017 0.017" (0.432 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Liner Design/Construction: Liner: PTFE Coated Fiberglass Side 1: Uncured Silicone Rubber Substrate: Laminated Tefzel® Substrate: Treated for adhesionThis data represents typical values for the productio.. |
|||
CTE, linear | 335 µm/m-°C | 186 µin/in-°F | Silicone Property; ASTM E 831 |
Arlon R37230R006 0.006" (0.152 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Substrate Design/Construction: Liner: FEP Add-on: Uncured Silicone Rubber Substrate: PTFE Coated Fiberglass This data represents typical values for the production material. The data should not be used to wri.. |
|||
CTE, linear | 335 µm/m-°C @Temperature 20.0 °C |
186 µin/in-°F @Temperature 68.0 °F |
silicone property; ASTM E 831 |
Arlon Thermabond® 99180T010 Silicone Rubber/Fiberglass Laminate Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass. |