Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 21.6 µm/m-°C @Temperature 20.0 °C |
12.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Owens Corning Glass Fiber Reinforced Polyester (Spray-up/Lay-up), 30 wt.% glass Data provided by the manufacturer, Owens Corning. |
|||
CTE, linear | 21.6 µm/m-°C @Temperature -40.0 - 149 °C |
12.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Ketron® GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
CTE, linear | 21.6 µm/m-°C | 12.0 µin/in-°F | ASTM D696 |
Quantum PEEK 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |
|||
CTE, linear | 21.6 µm/m-°C @Temperature 20.0 °C |
12.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylon® N1043HL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
CTE, linear | 21.6 µm/m-°C @Temperature 20.0 °C |
12.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylon® N1043L Nylon 6/6 (DAM) Information provided by Ravago. |
|||
CTE, linear | 21.6 µm/m-°C @Temperature 20.0 °C |
12.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Edgetek® PK-15CF-15GB/000 Polyetheretherketone (PEEK), Glass Bead, Carbon Fiber Reinforced
(discontin Description/Features:Carbon Fiber ReinforcedGlass Bead FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
CTE, linear | 21.6 µm/m-°C @Temperature 100 °C |
12.0 µin/in-°F @Temperature 212 °F |
ASTM E-831 (TMA) |
Technetics Group Amicon™ PEEK 30% Glass Filled
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
CTE, linear | 21.6 µm/m-°C @Temperature -40.0 - 149 °C |
12.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Ketron® GF30 LSG PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
CTE, linear | 21.6 - 119 µm/m-°C | 12.0 - 66.1 µin/in-°F | Average value: 54.1 µm/m-°C Grade Count:7 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
CTE, linear | 21.6 µm/m-°C @Temperature 20.0 °C |
12.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Edgetek® PF-40GF/000 Polysulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
CTE, linear | 21.6 µm/m-°C @Temperature -20.0 - 200 °C |
12.0 µin/in-°F @Temperature -4.00 - 392 °F |
ASTM D696 |
Ensinger ENSILON® 6/6 GF30 Extruded Nylon 6/6, 30% glass-fiber-reinforced (PA66)
(discontinued **) ENSILON 6/6 GF30 is a 30% glass-fiber-reinforced nylon 6/6 material whose important properties include high tensile and flexural strength, stiffness, excellent heat deflection, and superior abrasion.. |
|||
CTE, linear | 21.6 µm/m-°C @Temperature 20.0 °C |
12.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Firestone CG430-001 Nylon 6, 30% Fiberglass Filled Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.Information provided by Firestone |
|||
CTE, linear | 21.6 µm/m-°C @Temperature 20.0 °C |
12.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Firestone CG430-203 Nylon 6, 30% Fiberglass Filled Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.Information provided by Firestone |
|||
CTE, linear | 21.6 µm/m-°C @Temperature 20.0 °C |
12.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Techmer ES Electrafil® J-1200/CF/20 NAT ABS |
|||
CTE, linear | 21.6 µm/m-°C @Temperature 20.0 °C |
12.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Techmer ES Plaslube® J-1/CF/15/TF/20 NAT PA66 |
|||
CTE, linear | 21.6 µm/m-°C @Temperature 20.0 °C |
12.0 µin/in-°F @Temperature 68.0 °F |
|
Williams Advanced Alloys WS188 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
CTE, linear | 21.6 µm/m-°C @Temperature 20.0 °C |
12.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Lubrizol ESTALOC® T5160 Ether-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
CTE, linear | 21.6 µm/m-°C | 12.0 µin/in-°F | ASTM C531 |
Chesterton ARC 988 Composite Description: A high performance, quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by severe chemical and physi.. |
|||
CTE, linear | 21.6 µm/m-°C @Temperature 20.0 °C |
12.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ensinger Tecamid® GF30 Extruded Nylon 6/6 30% glass-fiber-reinforced (PA66) Tecamid® 6/6 GF30 is a 30% glass-fiber reinforced nylon 6/6 material whose important properties include high tensile and flexural strength, stiffness, excellent heat deflection temperature, and sup.. |
|||
CTE, linear | 21.6 µm/m-°C @Temperature 20.0 °C |
12.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK) Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent fle.. |
|||
CTE, linear | 21.6 - 28.8 µm/m-°C | 12.0 - 16.0 µin/in-°F | Average value: 24.0 µm/m-°C Grade Count:3 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |
|||
CTE, linear | 21.6 - 51.0 µm/m-°C | 12.0 - 28.3 µin/in-°F | Average value: 39.9 µm/m-°C Grade Count:15 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |
|||
CTE, linear | 21.6 - 110 µm/m-°C | 12.0 - 61.1 µin/in-°F | Average value: 66.6 µm/m-°C Grade Count:27 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |