Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 20.5 µm/m-°C @Temperature 23.0 - 60.0 °C |
11.4 µin/in-°F @Temperature 73.4 - 140 °F |
|
Sumitomo Bakelite Durez® 23570 Phenolic, Compression Grade Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft.. |
|||
CTE, linear | 20.5 µm/m-°C @Temperature 23.0 - 60.0 °C |
11.4 µin/in-°F @Temperature 73.4 - 140 °F |
|
Sumitomo Bakelite Durez® 23570 Phenolic, Injection Grade Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft.. |