Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 1.80 µm/m-°C @Temperature 649 °C |
1.00 µin/in-°F @Temperature 1200 °F |
|
Pyrotek Pyrocast AR-S Castable Refractory Pyrocast AR-S is a low cement, fused silica, castable refractory which exhibits excellent resistance to thermal shock. It is inert to liquid aluminum and its alloys. It is a high strength material.. |
|||
CTE, linear | 1.80 µm/m-°C @Temperature 100 - 1000 °C |
1.00 µin/in-°F @Temperature 212 - 1830 °F |
|
Pyrotek Pyrocast 220HT Refractory Castable Pyrocast 220HT is a high-performance refractory castable based on fused silica and silicon carbide.ApplicationsTransfer troughs Launder linings Filter boxes Pins and spouts AdvantagesThermal shock r.. |