Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 1.10 µm/m-°C @Temperature 20.0 - 100 °C |
0.611 µin/in-°F @Temperature 68.0 - 212 °F |
|
UCAR Carbon UCAR® CHV Extruded Graphite Typical uses for extruded grades are in the production of molds and crucibles, heating elements and furnace furniture, liquid metal processing equipment and chemical process equipment.Tabular proper.. |