Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 0.750 µm/m-°C @Temperature 0.000 - 300 °C |
0.417 µin/in-°F @Temperature 32.0 - 572 °F |
|
Corning Vycor® 7913 UV-Transmitting Glass Special Features:Superior optical qualityTight dimensional controlThermal and chemical properties ideally suited to high temperatures.Excellent thermal shock resistanceTypical Applications:Halogen l.. |
|||
CTE, linear | 0.750 µm/m-°C @Temperature 0.000 - 300 °C |
0.417 µin/in-°F @Temperature 32.0 - 572 °F |
|
Corning Vycor® 7950 Red Glass Used to reduce the light of quartz lamps (blocks most visible white light while transmitting IR). One specific use is blocking glare from heating units.Special Features:Superior optical qualityTigh.. |
|||
CTE, linear | 0.750 µm/m-°C @Temperature 0.000 - 300 °C |
0.417 µin/in-°F @Temperature 32.0 - 572 °F |
|
Corning Vycor® 7930 Porous Glass Open cell porous glass which exhibits excellent moisture absorbing properties ("thirsty"). It is mechanically hard and strong, nondusting, nonflaking, and chemically inert. These properties allow .. |