Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 0.710 - 146 µm/m-°C | 0.394 - 81.0 µin/in-°F | Average value: 44.4 µm/m-°C Grade Count:206 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |