Thermal Properties Metric English Comments
CTE, linear 9.00 - 9.60 µm/m-°C

@Temperature 20.0 - 100 °C
5.00 - 5.33 µin/in-°F

@Temperature 68.0 - 212 °F
MarkeTech Mo60Cu Moly/Copper Heat Sink Material
MoCu alloys are made by sintering molybdenum and copper together. This results in a heat sink of lower density than tungsten-based materials, low thermal expansion, and excellent thermal conductivit..