Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 17.0 - 70.4 µm/m-°C | 9.44 - 39.1 µin/in-°F | Average value: 38.7 µm/m-°C Grade Count:7 |
Overview of materials for PET + PBT Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |