Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | -1.00 - 7.00 µm/m-°C @Temperature 55.0 - 260 °C |
-0.556 - 3.89 µin/in-°F @Temperature 131 - 500 °F |
Average value: 2.88 µm/m-°C Grade Count:4 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
CTE, linear | -1.00 - 7.00 µm/m-°C @Thickness 2.00 - 4.00 mm |
-0.556 - 3.89 µin/in-°F @Thickness 0.0787 - 0.157 in |
Average value: 2.88 µm/m-°C Grade Count:4 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
CTE, linear | 6.30 - 7.00 µm/m-°C @Temperature 20.0 - 100 °C |
3.50 - 3.89 µin/in-°F @Temperature 68.0 - 212 °F |
|
MarkeTech W85Cu Tungsten/Copper Heat Sink Material WCu composites are made by vacuum infiltration of uniform controlled porous blocks of tungsten with molten copper. This results in a material with an interconnected Cu matrix that has high thermal c.. |
|||
CTE, linear | 6.00 - 7.00 µm/m-°C @Temperature 1000 °C |
3.33 - 3.89 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories BPSC-95 Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 5.00 - 7.00 µm/m-°C | 2.78 - 3.89 µin/in-°F | IPC TM-650 2.4.41 |
Arlon 45NK Woven Kevlar® Reinforced Laminate and Prepreg 45NK is a woven Kevlar® aramid fiber reinforced multifunctional epoxy laminate system engineered to provide in-plane CTE values as low as 6 ppm/°C for compatibility with leadless alumina ceramic c.. |