Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 20.0 - 67.0 µm/m-°C | 11.1 - 37.2 µin/in-°F | Average value: 39.6 µm/m-°C Grade Count:52 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
CTE, linear | 44.0 - 67.0 µm/m-°C @Temperature 40.0 - 130 °C |
24.4 - 37.2 µin/in-°F @Temperature 104 - 266 °F |
Average value: 54.0 µm/m-°C Grade Count:3 |
Overview of materials for Phenolic, Novolac, Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o.. |
|||
CTE, linear | 37.0 - 67.0 µm/m-°C @Temperature 40.0 - 130 °C |
20.6 - 37.2 µin/in-°F @Temperature 104 - 266 °F |
Average value: 56.6 µm/m-°C Grade Count:7 |
Overview of materials for Phenolic, Resole, Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Wood Filled". Each property range of values reported is minimum and maximum values of .. |
|||
CTE, linear | 28.8 - 67.0 µm/m-°C | 16.0 - 37.2 µin/in-°F | Average value: 54.8 µm/m-°C Grade Count:10 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
CTE, linear | 23.0 - 67.0 µm/m-°C | 12.8 - 37.2 µin/in-°F | Average value: 33.6 µm/m-°C Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |