Thermal Properties Metric English Comments
CTE, linear 50.4 - 63.0 µm/m-°C
28.0 - 35.0 µin/in-°F
Average value: 55.7 µm/m-°C Grade Count:6
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
CTE, linear 5.40 - 63.0 µm/m-°C
3.00 - 35.0 µin/in-°F
Average value: 37.7 µm/m-°C Grade Count:59
Overview of materials for Polyimide
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
CTE, linear 36.0 - 63.0 µm/m-°C
20.0 - 35.0 µin/in-°F
Average value: 49.7 µm/m-°C Grade Count:6
Overview of materials for Polypropylene, Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Wood Filled". Each property range of values reported is minimum and maximum values of app..