Thermal Properties Metric English Comments
CTE, linear 22.0 - 43.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
12.2 - 23.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics Lexan® LGK4030 PC (Asia Pacific)
CTE, linear 21.0 - 43.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.7 - 23.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL NC220 PPE+HIPS (Asia Pacific)
CTE, linear 25.0 - 43.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
13.9 - 23.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL NF1030 PPE+PS (Asia Pacific)
CTE, linear 20.0 - 43.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.1 - 23.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics NORYL GFN3L PPE+HIPS (Asia Pacific)
PPE+PS, GF30%, hydrolytic stability improved