Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 36.6 - 39.6 µm/m-°C @Temperature -60.0 - 60.0 °C |
20.3 - 22.0 µin/in-°F @Temperature -76.0 - 140 °F |
|
Mateck Potassium Bromide (KBr) Optical crystals |
|||
CTE, linear | 20.0 - 39.6 µm/m-°C | 11.1 - 22.0 µin/in-°F | Average value: 32.0 µm/m-°C Grade Count:15 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |