Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | -3.00 - 23.0 µm/m-°C | -1.67 - 12.8 µin/in-°F | Average value: 6.17 µm/m-°C Grade Count:5 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
CTE, linear | 1.00 - 23.0 µm/m-°C | 0.556 - 12.8 µin/in-°F | Average value: 5.74 µm/m-°C Grade Count:31 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
CTE, linear | 23.0 - 23.0 µm/m-°C @Temperature 140 - 180 °C |
12.8 - 12.8 µin/in-°F @Temperature 284 - 356 °F |
Average value: 23.0 µm/m-°C Grade Count:2 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |