Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 72.0 - 144 µm/m-°C | 40.0 - 80.0 µin/in-°F | Average value: 94.5 µm/m-°C Grade Count:17 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
CTE, linear | 6.00 - 144 µm/m-°C @Temperature 50.0 - 300 °C |
3.33 - 80.0 µin/in-°F @Temperature 122 - 572 °F |
Average value: 48.7 µm/m-°C Grade Count:29 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
CTE, linear | 54.0 - 144 µm/m-°C @Temperature 25.6 - 204 °C |
30.0 - 80.0 µin/in-°F @Temperature 78.0 - 400 °F |
ASTM D696 |
Technetics Group Texolon™ 9406 PTFE
(Unverified Data**) General purpose 25% glass filled PTFE for applications less demandingPTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Diel.. |
|||
CTE, linear | 54.0 - 144 µm/m-°C @Temperature 25.6 - 204 °C |
30.0 - 80.0 µin/in-°F @Temperature 78.0 - 400 °F |
ASTM D696 |
Garlock 9405 PTFE Rubber Sheet, 25% Glass Filled Premium Grade 25% Glass-filled Skived PTFE SheetInformation provided by Garlock Rubber Technologies |
|||
CTE, linear | 90.0 - 144 µm/m-°C @Temperature 20.0 °C |
50.0 - 80.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Zeus PVDF Tubing PVDF, polyvinylidene fluoride, delivers high performance at a competitive cost. Its inherent purity positions it as ideal for a variety of applications which involve extreme conditions. PVDF is char.. |
|||
CTE, linear | 119 - 144 µm/m-°C | 66.0 - 80.0 µin/in-°F | ASTM D696 |
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
CTE, linear | 119 - 144 µm/m-°C | 66.0 - 80.0 µin/in-°F | ASTM D696 |
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli.. |
|||
CTE, linear | 119 - 144 µm/m-°C | 66.0 - 80.0 µin/in-°F | ASTM D696 |
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha.. |
|||
CTE, linear | 119 - 144 µm/m-°C | 66.0 - 80.0 µin/in-°F | ASTM D696 |
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
CTE, linear | 119 - 144 µm/m-°C | 66.0 - 80.0 µin/in-°F | ASTM D696 |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |