Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 83.0 - 105 µm/m-°C @Temperature 23.0 - 60.0 °C |
46.1 - 58.3 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON NP-101 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: High speed wire and cable coatings.Information pro.. |
|||
CTE, linear | 83.0 - 105 µm/m-°C @Temperature 23.0 - 60.0 °C |
46.1 - 58.3 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON NP-120 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes.. |
|||
CTE, linear | 83.0 - 105 µm/m-°C @Temperature 23.0 - 60.0 °C |
46.1 - 58.3 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON NP-130 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Heavy wall wire insulation, cable jacketing, pipe, shrinka.. |
|||
CTE, linear | 83.0 - 105 µm/m-°C @Temperature 23.0 - 60.0 °C |
46.1 - 58.3 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON NP-21 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion .. |
|||
CTE, linear | 83.0 - 105 µm/m-°C @Temperature 23.0 - 60.0 °C |
46.1 - 58.3 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON NP-30 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing.. |
|||
CTE, linear | 83.0 - 105 µm/m-°C @Temperature 23.0 - 60.0 °C |
46.1 - 58.3 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON NP-40 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, transfer molding, compression molding.Applications: Films and s.. |
|||
CTE, linear | 83.0 - 105 µm/m-°C @Temperature 23.0 - 60.0 °C |
46.1 - 58.3 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON NP-20 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,.. |
|||
CTE, linear | 83.0 - 105 µm/m-°C @Temperature 23.0 - 60.0 °C |
46.1 - 58.3 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON NP-3000 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi.. |
|||
CTE, linear | 95.0 - 105 µm/m-°C @Temperature 20.0 °C |
52.8 - 58.3 µin/in-°F @Temperature 68.0 °F |
|
Abatron AboCast/AboCure 8109-10 2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro.. |