Thermal Properties Metric English Comments
CTE, linear -0.300 - 0.300 µm/m-°C

@Temperature 20.0 - 700 °C
-0.167 - 0.167 µin/in-°F

@Temperature 68.0 - 1290 °F
Schott ROBAX® Glass Ceramic
ROBAX® is a highly transparent glass-ceramic having virtually zero thermal expansion and sufficient mechanical resistance required for all standard applications. It is produced in flat, rolled s..