Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 95.0 µm/m-°C @Temperature 23.0 - 100 °C |
52.8 µin/in-°F @Temperature 73.4 - 212 °F |
|
Murtfeldt Murflor® + Bronze Polytetrafluoroethylene, 60% Bronze The addition of 60% bronze to the base material reduces the expansion coefficient and gives lower sliding wear.Special Properties:• Lower sliding wear than Murflor®• Good slide properties• Low s.. |
|||
CTE, linear | 95.0 µm/m-°C @Temperature 23.0 - 100 °C |
52.8 µin/in-°F @Temperature 73.4 - 212 °F |
|
Murtfeldt Murflor® Polytetrafluoroethylene, 25% Carbon The integration of 25% carbon increases the wear resistance, hardness, and creep strength of this material. Murflor® + Carbon is used, for example, when electrical conductivity is required and Mate.. |
|||
CTE, linear | 95.0 µm/m-°C @Temperature 23.0 - 100 °C |
52.8 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP Ertalon® 66 SA PA 66, extruded (ISO Data) Material with a higher mechanical strength, stiffness, heat and wear resistance than Ertalon 6 SA. It also has a better creep resistance but its impact strength and mechanical damping ability is red.. |
|||
CTE, linear | 95.0 µm/m-°C @Temperature 23.0 - 100 °C |
52.8 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP Nylatron® NSM PA 6 + internal lubricant, cast (ISO Data) Nylatron NSM is a proprietary cast nylon 6 formulation containing solid lubricant additives which grant this materials self-lubricity, excellent frictional behaviour, superior wear resistance and ou.. |
|||
CTE, linear | 95.0 µm/m-°C @Temperature 20.0 °C |
52.8 µin/in-°F @Temperature 68.0 °F |
Injection molded sample; ASTM D696 |
Ineos ABS Lustran® 456 Extrusion, Matte-Gloss
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
CTE, linear | 95.0 µm/m-°C @Temperature 20.0 °C |
52.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ineos ABS Lustran® 743 General Purpose, High-Impact
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La.. |
|||
CTE, linear | 95.0 µm/m-°C | 52.8 µin/in-°F | Conditioned 50% RH; ASTM D696 |
Manifattura Cattaneo PA 6.6 Nylon Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
CTE, linear | 95.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
52.8 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP101 Synthetic Fabric Description: Phenolic resin combined with spun nylon fabric. Good impact strength and excellent electrical properties under high humidity conditions. Meets applicable Boeing specification, but exemp.. |
|||
CTE, linear | 95.0 µm/m-°C @Temperature 20.0 °C |
52.8 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
LG Chemical NT-520 ABS, High Flow, Non Toxic Information Provided by LG Chem |
|||
CTE, linear | 95.0 µm/m-°C @Temperature 20.0 °C |
52.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Covestro Bayflex® MP-10000 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.118 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
CTE, linear | 95.0 µm/m-°C @Temperature 20.0 °C |
52.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Covestro Bayflex® MP-5000 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.118 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
CTE, linear | 95.0 - 105 µm/m-°C @Temperature 20.0 °C |
52.8 - 58.3 µin/in-°F @Temperature 68.0 °F |
|
Abatron AboCast/AboCure 8109-10 2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version.Pro.. |
|||
CTE, linear | 95.0 - 100 µm/m-°C @Temperature 20.0 °C |
52.8 - 55.6 µin/in-°F @Temperature 68.0 °F |
|
Abatron AboCast/AboCure 8109-4 Safety hardener (minimum toxicity) version of 8109-3.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 .. |
|||
CTE, linear | 95.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
52.8 µin/in-°F @Temperature -22.0 - 176 °F |
ASTM E228 |
Solvay Engineered Polymers DEXFLEX® 826HS TPO
(discontinued **) Description: DEXFLEX® 826HS is a thermoplastic olefinic elastomer (TPO) designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, and.. |
|||
CTE, linear | 95.0 - 153 µm/m-°C | 52.8 - 85.0 µin/in-°F | Average value: 123 µm/m-°C Grade Count:16 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |