Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.60 µm/m-°C | 4.78 µin/in-°F | at Set Pt. |
Ferro EG 4000 Display Device Glass Type: Pb-B (Composite) Typical Powder Form: VEG Typical Application: Seal Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and .. |
|||
CTE, linear | 8.60 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
4.78 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
CTE, linear | 8.60 µm/m-°C | 4.78 µin/in-°F | |
Anderman Ceramics EA995 Sintered Alumina, 99.5% Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |
|||
CTE, linear | 8.60 µm/m-°C | 4.78 µin/in-°F | |
Anderman Ceramics EA998 Sintered Alumina, 99.8% High purity fully dense alumina (99.8%) with high temperature capability of 1750°C. Available in rod, tube, plate, crucibles, sheaths and insulators up to 10 ft (3 m) long with diameters 0.3" to 1.. |
|||
CTE, linear | 8.60 µm/m-°C | 4.78 µin/in-°F | |
Anderman Ceramics EA99P Sintered Alumina, 99%, Porous Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |