Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.15 µm/m-°C @Temperature 260 °C |
4.53 µin/in-°F @Temperature 500 °F |
|
Ferro EG 4000 Display Device Glass Type: Pb-B (Composite) Typical Powder Form: VEG Typical Application: Seal Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and .. |
|||
CTE, linear | 8.15 µm/m-°C @Temperature 260 °C |
4.53 µin/in-°F @Temperature 500 °F |
|
Ferro EG 4010 Display Device Glass Type: Pb-B-AL Typical Powder Form: VSD Typical Application: Dielectric Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and pas.. |