Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 72.0 - 79.2 µm/m-°C | 40.0 - 44.0 µin/in-°F | ASTM D696 |
Quantum Nylon 6/6 Information provided by Quantum Advanced Engineering Plastics |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
NOVA Chemicals Laboratory Procedure |
NOVA Chemicals DYLARK® 238 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
CTE, linear | 72.0 - 90.0 µm/m-°C @Temperature 0.000 - 156 °C |
40.0 - 50.0 µin/in-°F @Temperature 32.0 - 312 °F |
Average value: 76.5 µm/m-°C Grade Count:4 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature -18.0 - 38.0 °C |
40.0 µin/in-°F @Temperature -0.400 - 100 °F |
ASTM D696 |
Plaskolite Optix® PL-150 Acrylic Resin
(discontinued **) Injection/extrusion pellets.Data provided by the manufacturer, Plaskolite, Inc. |
|||
CTE, linear | 72.0 - 160 µm/m-°C | 40.0 - 88.9 µin/in-°F | Average value: 88.1 µm/m-°C Grade Count:26 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech SP-3010 Rigid PVC Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
CTE, linear | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D 696 |
Styrolution PS 1900 GPPS Foam extrusionVery high flowHigh heat resistanceFree of zinc and oil additivesInformation provided by Styrolution |
|||
CTE, linear | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D 696 |
Styrolution PS 3100/3101 GPPS Good balance of flow and set-up propertiesModerate heat resistanceUSP Class VI certifiedInformation provided by Styrolution |
|||
CTE, linear | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D 696 |
Styrolution PS 3190/3191 GPPS Low residual styrene monomer contentGood balance of flow and set-up propertiesInformation provided by Styrolution |
|||
CTE, linear | 72.0 - 180 µm/m-°C | 40.0 - 100 µin/in-°F | |
TriStar Ultracomp UC-400 Composite Bearing Ultracomp UC-400 - Designed for high loads, low speeds, impact and vibration applications. UC-400 has a MOS2 additive for salt water applications where cathodic reactions could occur. Excellent dry .. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 8132 Rigid PVC, Extrusion Georgia Gulf 8132 is a rigid PVC compound designed for applications where transparency is important. This product remains unchanged except for the coded name and was previously identified as 3132. .. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 8150 Rigid PVC, Extrusion & Molding Georgia Gulf 8150 is a special purpose rigid PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChemical Resista.. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 8264 Rigid PVC, Extrusion Georgia Gulf 8264 is a rigid PVC pellet compound suited for applications where transparency is important. 8264 is widely used for clear films, sheets, and profile shapes in the packaging industry. .. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 3240 Rigid PVC, Extrusion Georgia Gulf 3240 is a special purpose rigid powder blend PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChe.. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ensinger ENSIFIDE® PPS (Polyphenylene Sulfide) - Extruded Products
(discontinued **) ENSIFIDE is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves ENSIFIDE at.. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 6511 Rigid PVC, Molding Georgia Gulf 6511 is a special purpose rigid PVC compound designed for applications requiring the following properties: GlossImpact Strength & ToughnessFlame RetardantChemical ResistantThermoformab.. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Spectar® UV Copolyester Sheet Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech. |