Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 7.60 µm/m-°C | 4.22 µin/in-°F | |
Poco Graphite ACF-10Q Industrial Grade Graphite POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr.. |
|||
CTE, linear | 7.60 µm/m-°C | 4.22 µin/in-°F | |
Poco Graphite AXZ-5Q Industrial Grade Graphite POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr.. |
|||
CTE, linear | 7.60 µm/m-°C | 4.22 µin/in-°F | |
Poco Graphite SCF Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
CTE, linear | 7.60 µm/m-°C | 4.22 µin/in-°F | |
Poco Graphite SCF-2 Ion Implant Grade Graphite An economic alternative to DFP-3-2, this 5-micron material is harder than DFP-3-2 and has high strengths without reduced porosity. |
|||
CTE, linear | 7.60 µm/m-°C @Temperature 20.0 °C |
4.22 µin/in-°F @Temperature 68.0 °F |
|
MarkeTech Aluminum Oxide Ceramic - Alumina 97.5% Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture.. |
|||
CTE, linear | 7.60 µm/m-°C @Temperature 20.0 °C |
4.22 µin/in-°F @Temperature 68.0 °F |
|
GBC Grade 97 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
CTE, linear | 7.60 µm/m-°C @Temperature 20.0 - 100 °C |
4.22 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals NI-SPAN-C® Alloy 902 A nickel-iron-chromium alloy made precipitation hardenable by additions of aluminum and titanium. The titanium content also helps provide a controllable thermoelastic coefficient, which is the allo.. |
|||
CTE, linear | 7.60 µm/m-°C @Temperature 20.0 °C |
4.22 µin/in-°F @Temperature 68.0 °F |
|
Sapco 95% Aluminum Oxide Information provided by Sapco. |
|||
CTE, linear | 7.60 - 8.50 µm/m-°C @Temperature 25.0 - 800 °C |
4.22 - 4.72 µin/in-°F @Temperature 77.0 - 1470 °F |
|
China-Yixing Longly Refractories 99 Alumina Ceramic Seals LONGLY's alumina ceramic seals (alumina accounts for 95-99%) can be finished by mirror-polishing process. Because of high mechanical strength, strong chemical corrosion resistance, good air tightne.. |
|||
CTE, linear | 7.60 µm/m-°C @Temperature 20.0 °C |
4.22 µin/in-°F @Temperature 68.0 °F |
|
CMW® THERMKON® 76 Tungsten Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
CTE, linear | 7.60 - 8.50 µm/m-°C @Temperature 25.0 - 800 °C |
4.22 - 4.72 µin/in-°F @Temperature 77.0 - 1470 °F |
|
China-Yixing Longly Refractories 99 Alumina Ceramic LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, .. |