Thermal Properties Metric English Comments
CTE, linear 6.10 µm/m-°C

@Temperature 20.0 °C
3.39 µin/in-°F

@Temperature 68.0 °F
Pyrotek Valcor® G-AZ Pre-Cast Shapes
ApplicationsBurner blocks Skimmer blocks Cover blocks Specialty blocks Plungers Stirrers Spouts Feeder tubes AdvantagesProven performance in molten glass contact applications Smooth surface finish d..
CTE, linear 6.10 µm/m-°C
3.39 µin/in-°F
at Set Pt. (Fired Thermal Expansion)
Ferro CF 7578 Low-Temperature Sealing
DEVITRIFYING Typical Powder Form: VSD Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific ..
CTE, linear 6.10 µm/m-°C

@Temperature 20.0 °C
3.39 µin/in-°F

@Temperature 68.0 °F
CMW® THERMKON® 62 Tungsten Copper parts
For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc.
CTE, linear 6.10 µm/m-°C

@Temperature 20.0 - 1093 °C
3.39 µin/in-°F

@Temperature 68.0 - 1999 °F
BNZ Materials BNZ-28 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
CTE, linear 6.10 µm/m-°C

@Temperature 20.0 - 1093 °C
3.39 µin/in-°F

@Temperature 68.0 - 1999 °F
BNZ Materials BNZ-3000 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
CTE, linear 6.10 µm/m-°C

@Temperature 20.0 - 1093 °C
3.39 µin/in-°F

@Temperature 68.0 - 1999 °F
BNZ Materials BNZ-32 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
CTE, linear 6.10 µm/m-°C

@Temperature 27.0 - 175 °C
3.39 µin/in-°F

@Temperature 80.6 - 347 °F
ASTM D696
3M 7945MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
CTE, linear 6.10 µm/m-°C

@Temperature 27.0 - 175 °C
3.39 µin/in-°F

@Temperature 80.6 - 347 °F
ASTM D696