Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 55.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
30.6 µin/in-°F @Temperature -22.0 - 176 °F |
ASTM E228 |
Solvay Engineered Polymers SEQUEL® 1718HF Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1718HF engineered polyolefin is designed for painted automotive exterior applications that require dimensional stability over a broad temperature range. This material exhibits.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
30.6 µin/in-°F @Temperature -22.0 - 176 °F |
ASTM E228 |
Solvay Engineered Polymers SEQUEL® 1733HI Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1733HI engineered polyolefin is designed for large, painted automotive exterior applications that require dimensional stability over a broad temperature range. This material e.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
30.6 µin/in-°F @Temperature -22.0 - 176 °F |
ASTM E228 |
Solvay Engineered Polymers SEQUEL® 1783 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1783 engineered polyolefin is designed for large, mold-in-color automotive exterior applications that require dimensional stability over a broad temperature range. This materi.. |
|||
CTE, linear | 55.0 - 75.0 µm/m-°C | 30.6 - 41.7 µin/in-°F | Polykemi |
Polykemi AB POLYfill PP EIP12030RF Polypropylene/EPDM, Mineral Reinforced Information provided by Polykemi AB |
|||
CTE, linear | 55.0 - 65.0 µm/m-°C | 30.6 - 36.1 µin/in-°F | Polykemi |
Polykemi AB POLYfill PP HJ752 Polypropylene/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
CTE, linear | 55.0 µm/m-°C | 30.6 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1500-8299 Polysulfone, with PTFE, lubricant modified Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca.. |
|||
CTE, linear | 55.0 µm/m-°C | 30.6 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1502-7867/BL4 PPSU, unreinforced Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature 20.0 °C |
30.6 µin/in-°F @Temperature 68.0 °F |
Vertical Direction; ASTM D696 |
Mitsui Arlen™ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature 20.0 °C |
30.6 µin/in-°F @Temperature 68.0 °F |
Vertical Direction; ASTM D696 |
Mitsui Arlen™ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
CTE, linear | 55.0 µm/m-°C | 30.6 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1100-7939/GY Polyether sulfone, unreinforced Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature 20.0 °C |
30.6 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Stratasys® Polyphenylsulfone PPSF/PPSU (polyphenylsulfone) material has the greatest strength, heat and chemical resistance of all Stratasys materials - ideal for aerospace, automotive and medical applications. Stratasys FDM (F.. |
|||
CTE, linear | 55.0 µm/m-°C | 30.6 µin/in-°F | ASTM D696 |
Samyang Trirex® 3025N1 Polycarbonate, Flame Retardant TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
CTE, linear | 55.0 µm/m-°C | 30.6 µin/in-°F | Absolute Drying; ASTM-D696 |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature 20.0 °C |
30.6 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Bond 2135D High Impact Epoxy Adhesive TRA-BOND 2135D is a medium viscosity epoxy adhesive recommended for bonding, laminating, sealing, and structural repair applications where easy mixing and good wetting combined with high impact stre.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature 20.0 °C |
30.6 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Bond 2105 Clear Rigid, Medium Viscosity Epoxy Adhesive TRA-BOND 2105 is a clear, medium viscosity epoxy adhesive which contains no solvents or other additives which can be harmful to the environment or to its users. It has excellent adhesion to glass, c.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature 20.0 °C |
30.6 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Bond 2115 Clear High Strength Epoxy Adhesive TRA-BOND 2115 is a clear, low viscosity epoxy formulation used in the fabrication of lasers. It is capable of withstanding 30 seconds of 60 watt direct laser energy. The low cure shrinkage (using a .. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
30.6 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
CP-Polymer-Technik Wellamid® 6000 MR 409 HWCP Mineral Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
CTE, linear | 55.0 µm/m-°C | 30.6 µin/in-°F | |
Hippe PA 6 Nylon 6 Very tough, even at low temperatures. Hard. High attenuation properties. Technical components such as gear wheels, pinions, screws, nuts, bearings, seals, cloth components, guide components, pump.. |
|||
CTE, linear | 55.0 - 65.0 µm/m-°C @Temperature 20.0 °C |
30.6 - 36.1 µin/in-°F @Temperature 68.0 °F |
|
Abatron AboCast/AboCure 8109-5 High heat resistance. Easy to use.Processing: 100/20 pbw; Potlife: 7-10 days/20°C (68°F), 5-7h/60°C (140°F); mix at RT; cures in: 4 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applications.. |
|||
CTE, linear | 55.0 - 65.0 µm/m-°C @Temperature 20.0 °C |
30.6 - 36.1 µin/in-°F @Temperature 68.0 °F |
|
Abatron AboCast/AboCure 8109-6 High heat resistance. Easy to use.Processing: 100/90 pbw; Potlife: 15-20 days/20°C (68°F), 7-10 h/120°C (250°F); mix at RT; cures in: 3 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applicat.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature 20.0 °C |
30.6 µin/in-°F @Temperature 68.0 °F |
|
Armstrong A-2/E Epoxy Adhesive This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac.. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature 20.0 °C |
30.6 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Chang Chun Plastic PBT4815 Fire Retardant & 15% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
30.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
Beijing Chemical Industry KAIFA® 201-G20R PBT Resin 15% glass fiber reinforced, good flow and toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
CTE, linear | 55.0 - 65.0 µm/m-°C | 30.6 - 36.1 µin/in-°F | Polykemi |
Polykemi AB POLYfill PPH BF405510 VT1 Polypropylene Homopolymer, Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
CTE, linear | 55.0 µm/m-°C @Temperature 20.0 °C |
30.6 µin/in-°F @Temperature 68.0 °F |
Vertical Direction; ASTM D696 |
Mitsui Arlen™ C215 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses .. |
|||
CTE, linear | 55.0 - 65.0 µm/m-°C @Temperature 20.0 °C |
30.6 - 36.1 µin/in-°F @Temperature 68.0 °F |
|
Abatron AboCast/AboCure 8109-7 Processing: 100/80 pbw; Potlife: 6-7 days/20°C (68°F), 12-24 h/40°C (105°F), 0.75-7 h /60°C (140°F); mix at 50-80°C (120-175°F); cures in: 1 h/100°C (212°F) + 4 h/150°C (300°F) postcure... |
|||
CTE, linear | 55.0 µm/m-°C | 30.6 µin/in-°F | ASTM E831 |
Addiplast Addinyl PMD 20170 Nylon 66 GalvanizingInformation provided by Addiplast. |
|||
CTE, linear | 55.0 µm/m-°C @Temperature 23.0 - 100 °C |
30.6 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP Quadrant PSU unfilled, extruded (ISO Data) Quadrant 1000 PSU is a slightly yellow, translucent (non-optical quality) amorphous thermoplastic material, offering a combination of excellent mechanical, thermal and electrical properties. It ofte.. |