Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
|
North Wood Plastics Polypropylene with 40% Wood Fiber, Extrusion Grade Data provided by North Wood Plastics, Inc. |
|||
CTE, linear | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
|
North Wood Plastics Polypropylene with 40% Wood Fiber, Molding Grade Data provided by North Wood Plastics, Inc. |
|||
CTE, linear | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
ASTM E228 |
Solvay Engineered Polymers SEQUEL® 2380 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 2380 engineered polyolefin is designed for large mold-in-color automotive interior applications that require stiffness and dimensional stability over a broad temperature range... |
|||
CTE, linear | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
NOVA |
NOVA Chemicals Dylark® 250P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
CTE, linear | 50.0 - 70.0 µm/m-°C @Temperature 20.0 °C |
27.8 - 38.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Kolon Kocetal® WH702 Reinforced Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
CTE, linear | 50.0 - 110 µm/m-°C | 27.8 - 61.1 µin/in-°F | Average value: 68.2 µm/m-°C Grade Count:24 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
CTE, linear | 50.0 µm/m-°C | 27.8 µin/in-°F | Below Tg |
EVALCA EVAL® EP-F104BW Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, blow molding, tubes, coex coating. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL.. |
|||
CTE, linear | 50.0 µm/m-°C | 27.8 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 50/GF/10/TF/18/SI/2/GY5 Polycarbonate, with glass fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
CTE, linear | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
Vertical Direction; ASTM D696 |
Mitsui Arlen™ C230 30% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
CTE, linear | 50.0 µm/m-°C @Temperature -30.0 - 100 °C |
27.8 µin/in-°F @Temperature -22.0 - 212 °F |
ASTM D696 |
LyondellBasell Hifaxâ„¢ BB222GC Thermoplastic Olefin Resin Key Features: medium melt flow, very high modulus, UV-stabilized thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, excellent weatherability, high stiffness, good dimens.. |
|||
CTE, linear | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
|
Trelleborg Emerson & Cuming Stycast® 2057/9 Two-Component General Purpose Encapsulant Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as .. |
|||
CTE, linear | 50.0 µm/m-°C | 27.8 µin/in-°F | MIL STD 883D |
CoorsTek Epoxy Seal 216 (ES-216) B-staged epoxy lids ES-216 is available for applications where high strength and moisture resistance are required. It displays fillet formation characteristics and, after cure, is highly temperature and moisture resist.. |
|||
CTE, linear | 50.0 - 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 - 50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON EP-521 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
CTE, linear | 50.0 - 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 - 50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON RP-5000AS EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
CTE, linear | >= 50.0 µm/m-°C | >= 27.8 µin/in-°F | |
Epoxyset Epoxibond EB-119SP Unfilled Epoxy Adhesive A two-component, unfilled, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc... |
|||
CTE, linear | 50.0 µm/m-°C | 27.8 µin/in-°F | |
Hippe PPS High hardness and stiffness, good abrasion resistance, low moisture absorption, favorable insulating features, low dielectric, high non-inflammability and high chemical resistance are the essential .. |
|||
CTE, linear | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
E-Polymers TEKAMID® TB120G15T Impact Modified, 15% Glass Fiber Reinforced PA6, DAM 15% GF reinforced, Good impact resistanceInformation provided by E-Polymers Co. Ltd. |
|||
CTE, linear | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Covestro Bayflex® XGT-100 Polyurethane Elastomeric RIM, 15% Milled Glass Filled, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
CTE, linear | 50.0 - 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 - 50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON EP-620 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
CTE, linear | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Chang Chun Plastic PBT3015 15% Glass Fiber Enforced PBT Information provided by Dowell Trading Company Ltd. |
|||
CTE, linear | 50.0 - 75.0 µm/m-°C | 27.8 - 41.7 µin/in-°F | Polykemi |
Polykemi AB POLYfill PPH TS5040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
CTE, linear | 50.0 µm/m-°C | 27.8 µin/in-°F | ASTM D696 |
Gromax PBT 4115-201D 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
CTE, linear | 50.0 µm/m-°C @Temperature 20.0 - 100 °C |
27.8 µin/in-°F @Temperature 68.0 - 212 °F |
|
Isoflon PCTFE Polychlorotrifluoroethylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
CTE, linear | 50.0 µm/m-°C | 27.8 µin/in-°F | DIN 53752 |
Lehmann & Voss PLASLUBE J-50/10/TF/15/BK Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |