Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 5.35 µm/m-°C @Temperature 100 °C |
2.97 µin/in-°F @Temperature 212 °F |
|
CMW® ELKON 100M Pure Molybdenum Molybdenum (ELKON® 100M) is a refractory metal that resembles tungsten in many respects. Its hardness, melting, and boiling temperatures are only slightly lower than those of tungsten are. The elec.. |