Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 46.8 µm/m-°C @Temperature -40.0 - 150 °C |
26.0 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E831 |
Quadrant EPP Ketron® 1000 IM Injection Molded Unfilled Polyetheretherketone (ASTM Product Data Sheet) Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam |
|||
CTE, linear | 46.8 µm/m-°C @Temperature -40.0 - 149 °C |
26.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Ketron® 1000 LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet) |
|||
CTE, linear | 46.8 µm/m-°C @Temperature -40.0 - 149 °C |
26.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet) |
|||
CTE, linear | 46.8 µm/m-°C @Temperature 100 °C |
26.0 µin/in-°F @Temperature 212 °F |
ASTM E-831 (TMA) |
Technetics Group Amicon™ PEEK
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
CTE, linear | 46.8 µm/m-°C @Temperature -40.0 - 149 °C |
26.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Duratron® PAI T5530 Compression Molded Glass Reinforced Polyamide-imide (ASTM Product Data Sheet) |
|||
CTE, linear | 46.8 µm/m-°C @Temperature 20.0 °C |
26.0 µin/in-°F @Temperature 68.0 °F |
modified; ASTM D696 |
LyondellBasell SEQUEL® E5000 TPO Description: SEQUEL® E5000 thermoplastic olefinic elastomer (TPO) is designed for extrusion applications that require high mechanical stiffness, thermal stability, good low-temperature properties.. |
|||
CTE, linear | 46.8 µm/m-°C @Temperature 20.0 °C |
26.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics PEEK PEEK is a high performance semi-crystalline thermoplastic. PEEK characteristics include high temperature performance, excellent wear properties, superior chemical resistance and outstanding toughne.. |
|||
CTE, linear | 46.8 µm/m-°C | 26.0 µin/in-°F | |
Hexcel® F161 Epoxy Resin F161 is a structural, heat resistant and electrical grade epoxy formulation designed for autoclave curing. F161 is a high temperature, laminate grade epoxy resin with a 350ºF (177ºC) cure. F161 is.. |
|||
CTE, linear | 46.8 µm/m-°C | 26.0 µin/in-°F | ASTM C531 |
Chesterton ARC 855 Abrasion Control Liquid Description: An advanced ceramic composite formulated to protect equipment from aggressive chemical attack, corrosion, and erosion. The product is a low viscosity composite that is easily applied by.. |
|||
CTE, linear | 46.8 µm/m-°C | 26.0 µin/in-°F | ASTM D696 |
Ensinger Tecapeek® Classix Polyaryletherketone (PAEK) TECAPEEK™ high performance polymer has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's exceptional combination of properties al.. |
|||
CTE, linear | 46.8 µm/m-°C | 26.0 µin/in-°F | ASTM D696 |
Ensinger Tecapeek® MT Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
CTE, linear | 46.8 µm/m-°C @Temperature 20.0 °C |
26.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ensinger Tecapeek® Polyetheretherketone (PEEK) Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance.Excellent flex.. |
|||
CTE, linear | 46.8 µm/m-°C | 26.0 µin/in-°F | ASTM D696 |
Ensinger Tecapeek® Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
CTE, linear | 46.8 µm/m-°C @Temperature 20.0 °C |
26.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Kasei Thermylene® F6-30FG-0100 30% Glass Fiber Reinforced, Chemically Coupled Information provided by Asahi Thermofil |
|||
CTE, linear | 46.8 µm/m-°C | 26.0 µin/in-°F | ASTM D696 |
Teknor Apex Chemlon® 140 MH Nylon 66, 40% Mineral Reinforced Notes: 40% Mineral; High rigidity with exceptional control of warpage and surface sink marks; Excellent for large parts; Fast cycling Features: Fast Molding Cycle; High Rigidity; Heat Stabilized; Lo.. |
|||
CTE, linear | 46.8 µm/m-°C | 26.0 µin/in-°F | ASTM D696 |
Quantum PEEK Information provided by Quantum Advanced Engineering Plastics |