Polymer Property : CTE, linear = 38.3 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 38.3 - 101 µm/m-°C
21.3 - 56.0 µin/in-°F
Average value: 79.9 µm/m-°C Grade Count:8
Overview of materials for PVC/Acrylic Alloy
This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate ..
CTE, linear 38.3 µm/m-°C

@Temperature 20.0 °C
21.3 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Kleerdex Kydex® 510 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Weatherable and decorative sheetApplications: Housings for equipment, recreation vehicles and truck parts, safety equipment, building products, signage, wall panels, facia, doors, service counters, ..