Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 3.70 µm/m-°C @Temperature 25.0 - 260 °C |
2.06 µin/in-°F @Temperature 77.0 - 500 °F |
|
Ferro IP 900 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Si-Pb-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
CTE, linear | 3.70 µm/m-°C | 2.06 µin/in-°F | at Set Pt.; Crystallized |
Ferro IX 2730 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: TF Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures and can.. |
|||
CTE, linear | 3.70 µm/m-°C @Temperature 20.0 - 900 °C |
2.06 µin/in-°F @Temperature 68.0 - 1650 °F |
after initial firing |
Zircar Ceramics Z-500 Alumina-Silica Insulation Useful to temperatures of 1000°C (1832°F) Z-500 is uniformly rigidized and hard throughout its entire thickness, requiring no re-rigidizing after precision machining into complex shapes and confia.. |
|||
CTE, linear | 3.70 µm/m-°C @Temperature 1000 °C |
2.06 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CRAG-S27 Long Stopper Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |