Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 28.8 µm/m-°C @Temperature 20.0 °C |
16.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylon® N1033THL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
CTE, linear | 28.8 - 110 µm/m-°C | 16.0 - 61.1 µin/in-°F | Average value: 85.4 µm/m-°C Grade Count:32 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
CTE, linear | 28.8 - 54.0 µm/m-°C | 16.0 - 30.0 µin/in-°F | Average value: 40.3 µm/m-°C Grade Count:5 |
Overview of materials for ABS/Polyester Alloy + GF This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro.. |
|||
CTE, linear | 28.8 µm/m-°C @Temperature 20.0 °C |
16.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Edgetek® AS-30GF/000 FRVO Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFlame RetardantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
CTE, linear | 28.8 µm/m-°C @Temperature 20.0 °C |
16.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylon® N1033TL Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
CTE, linear | 28.8 - 67.0 µm/m-°C | 16.0 - 37.2 µin/in-°F | Average value: 54.8 µm/m-°C Grade Count:10 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
CTE, linear | 28.8 µm/m-°C @Temperature 20.0 °C |
16.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Edgetek® SF-20GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
CTE, linear | 28.8 µm/m-°C @Temperature 100 °C |
16.0 µin/in-°F @Temperature 212 °F |
|
Greene Tweed AR™ HT Abrasive-Resistant Thermoplastic ARHT™ is a proprietary thermoplastic material specifically developed for use a sbushings, bearings and wear rings in pumps handling abrasive media up to 250°F (121°C). ARHT provides outs.. |
|||
CTE, linear | 28.8 µm/m-°C @Temperature 20.0 °C |
16.0 µin/in-°F @Temperature 68.0 °F |
ASTM D1525 |
PlastxWorld CEVIAN® S1230 PC/ABS alloy Glass fiber reinforced PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
CTE, linear | 28.8 µm/m-°C | 16.0 µin/in-°F | ASTM D696 |
Ensinger HYDLAR® Z Nylon, Pultruded Aramid Fiber Reinforced (PA) HYDLAR® possesses a combination of physical properties that cannot be found in any other commercially available engineered plastic. Design engineers have created a family of superior wear and abra.. |
|||
CTE, linear | 28.8 µm/m-°C @Temperature 20.0 °C |
16.0 µin/in-°F @Temperature 68.0 °F |
|
Aremco Aremco-Bond™ 820 High Performance Epoxide Clear, 1:1, 45-Minute Cure System with Good Flexibility |
|||
CTE, linear | 28.8 µm/m-°C @Temperature 20.0 °C |
16.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Edgetek® NI-30GF/000 Nylon 6/10 - 30% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |