Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 18.9 µm/m-°C @Temperature 20.0 - 649 °C |
10.5 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Eagle Brass 305 Austenitic Stainless Steel, 1/2 Hardened Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. .. |
|||
CTE, linear | 18.9 µm/m-°C @Temperature 20.0 - 649 °C |
10.5 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Eagle Brass 305 Austenitic Stainless Steel, 1/4 Hardened Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. .. |
|||
CTE, linear | 18.9 µm/m-°C @Temperature 20.0 - 649 °C |
10.5 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Eagle Brass 305 Austenitic Stainless Steel, Annealed Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. .. |