Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 17.8 µm/m-°C @Temperature 20.0 - 300 °C |
9.90 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 510 Phosphor Bronzes 5% A, 1/2 Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
CTE, linear | 17.8 µm/m-°C @Temperature 20.0 - 300 °C |
9.90 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 510 Phosphor Bronzes 5% A, 1/4 Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
CTE, linear | 17.8 µm/m-°C @Temperature 20.0 - 300 °C |
9.90 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 510 Phosphor Bronzes 5% A, 3/4 Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
CTE, linear | 17.8 µm/m-°C @Temperature 20.0 - 300 °C |
9.90 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 510 Phosphor Bronzes 5% A, Annealed Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
CTE, linear | 17.8 µm/m-°C @Temperature 20.0 - 300 °C |
9.90 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
CTE, linear | 17.8 µm/m-°C @Temperature 20.0 - 300 °C |
9.90 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Spring Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
CTE, linear | 17.8 µm/m-°C @Temperature 20.0 - 300 °C |
9.90 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 510 Phosphor Bronzes 5% A, Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
CTE, linear | 17.8 µm/m-°C @Temperature 20.0 - 300 °C |
9.90 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 510 Phosphor Bronzes 5% A, Spring Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
CTE, linear | 17.8 µm/m-°C @Temperature 20.0 - 300 °C |
9.90 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 511 Phosphor Bronzes 4%, 1/2 Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
CTE, linear | 17.8 µm/m-°C @Temperature 20.0 - 300 °C |
9.90 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 511 Phosphor Bronzes 4%, 1/4 Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
CTE, linear | 17.8 µm/m-°C @Temperature 20.0 - 300 °C |
9.90 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 511 Phosphor Bronzes 4%, 3/4 Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
CTE, linear | 17.8 µm/m-°C @Temperature 20.0 - 300 °C |
9.90 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 511 Phosphor Bronzes 4%, Annealed 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
CTE, linear | 17.8 µm/m-°C @Temperature 20.0 - 300 °C |
9.90 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 511 Phosphor Bronzes 4%, Extra Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
CTE, linear | 17.8 µm/m-°C @Temperature 20.0 - 300 °C |
9.90 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 511 Phosphor Bronzes 4%, Extra Spring 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
CTE, linear | 17.8 µm/m-°C @Temperature 20.0 - 300 °C |
9.90 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 511 Phosphor Bronzes 4%, Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
CTE, linear | 17.8 µm/m-°C @Temperature 20.0 - 300 °C |
9.90 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 511 Phosphor Bronzes 4%, Spring 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
CTE, linear | 17.8 µm/m-°C | 9.90 µin/in-°F | ASTM-D696 |
CoorsTek PolyGlyde™ 3000 Self-Lubricating Seal PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni.. |
|||
CTE, linear | 17.8 µm/m-°C @Temperature 100 °C |
9.89 µin/in-°F @Temperature 212 °F |
|
CMW® 73 Copper Alloy CMW® 73 material is a heat treatable copper base alloy having extremely high hardness and strength coupled with fair electrical and thermal conductivity. The extremely high hardness, strength and w.. |