Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 15.6 µm/m-°C @Temperature 20.0 °C |
8.67 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Lubrizol ESTALOC® 59600 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
CTE, linear | 15.6 µm/m-°C @Temperature 20.0 °C |
8.67 µin/in-°F @Temperature 68.0 °F |
|
California Fine Wire Stablohm 610 Nickel, Chromium and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
CTE, linear | 15.6 µm/m-°C @Temperature 25.0 - 100 °C |
8.67 µin/in-°F @Temperature 77.0 - 212 °F |
ASTM E831 |
M Cubed Technologies ASC-301 Aluminum alloy-30% SiC Metal Matrix Composite High stiffness, low density composite. Parts are cast using several standard foundry techniques Size range varies from small components (1lb or smaller) to parts greater than 10 ft. square with co.. |