Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
78.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Owens Corning Glass Fiber Reinforced Polyurethane, Milled Fibers (RRIM), 13 wt.% glass Polyurethane is normally used for its structural properties when molded. It is highly resistant to most organic solvents. It is not recommended for use with strong acids and alkalis, steam, fuels, a.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 23.0 - 100 °C |
77.8 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP Borotron® HM PE-HMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
NOVA Chemicals Novapol® HD-2007-H HDPE Extrusion Resin Features: Excellent ESCR and toughness, high strength, excellent processability, very high melt strength.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provid.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
NOVA Chemicals Novapol® HD-2100-U MDPE Extrusion Resin Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
78.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylon® N1000STHL Nylon 6/6 (DAM) Information provided by Ravago |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
NOVA Chemicals Novapol® PP-0118-F LLDPE Extrusion Resin Excellent ESCR, Excellent toughness, High strength, High flexibilityApplications: Pipes for pressure and non-pressure service from 12 mm to 100 mm, Potable water pipe and tubing, Underground sprinkl.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
|
3M Dyneon™ Fluorel™ Dipolymer, 22% Carbon Black Filled
(discontinued **) Data provided by the manufacturer, Dyneon LLC.66% fluorine content. See the many specific grades of Fluorel™ fluoroelastomer in MatWeb. |
|||
CTE, linear | 140 µm/m-°C @Temperature -20.0 - 32.0 °C |
77.8 µin/in-°F @Temperature -4.00 - 89.6 °F |
ASTM D696 |
DuPont™ Surlyn® 8527 Ionomer Resin, Sodium
(discontinued **) Surlyn® 8527 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
CTE, linear | 140 - 250 µm/m-°C @Temperature 100 - 200 °C |
77.8 - 139 µin/in-°F @Temperature 212 - 392 °F |
Average value: 195 µm/m-°C Grade Count:1 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo Pelprene™ P-280B Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo PELPRENE™ P90B Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo PELPRENE™ S2001 Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo PELPRENE™ S2002 Polyester TPE, Ultra Heat-resistant Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo PELPRENE™ S9001 Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo PELPRENE™ S9002 Polyester TPE, Ultra Heat-resistant Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo. |
|||
CTE, linear | 140 µm/m-°C @Temperature 23.0 - 55.0 °C |
77.8 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® SF-20 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 140 µm/m-°C | 77.8 µin/in-°F | Above Tg |
Tra-Con Tra-Bond 789-3TN1 Moisture Resistant Adhesive TRA-BOND 789-3TN1 adhesive is a thixotropic version of TRA-BOND 789-3. It is a one component, high strength, toughened adhesive designed for use in applications which require good moisture resistanc.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
|
Cytec EN-2543 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
CTE, linear | 140 µm/m-°C @Temperature -20.0 - 32.0 °C |
77.8 µin/in-°F @Temperature -4.00 - 89.6 °F |
ASTM D696 |
DuPont™ Surlyn® 8920 Ionomer Resin, Sodium Surlyn® 8920 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
CTE, linear | 140 µm/m-°C @Temperature -20.0 - 32.0 °C |
77.8 µin/in-°F @Temperature -4.00 - 89.6 °F |
ASTM D696 |
DuPont™ Surlyn® PC100 Ionomer Resin, Highest Clarity, Sodium Surlyn® PC100 luxury molding resin is a "select" grade of Surlyn® 8920, controlled to achieve the highest possible optical clarity in molded perfume jars and caps. It complies with the provisions .. |
|||
CTE, linear | 140 µm/m-°C | 77.8 µin/in-°F | |
Fainplast Compounds EVAtech 803S Ethylene Vinyl Acetate Foam EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds |
|||
CTE, linear | 140 µm/m-°C @Temperature -40.0 - 140 °C |
77.8 µin/in-°F @Temperature -40.0 - 284 °F |
ASTM D696 |
Arkema Group Pebax® 6333 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
CTE, linear | 140 - 160 µm/m-°C @Temperature 20.0 °C |
77.8 - 88.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer
(discontinued **) Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD.. |
|||
CTE, linear | 140 - 190 µm/m-°C | 77.8 - 106 µin/in-°F | Average value: 163 µm/m-°C Grade Count:8 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |
|||
CTE, linear | 140 - 140 µm/m-°C @Temperature 60.0 - 138 °C |
77.8 - 77.8 µin/in-°F @Temperature 140 - 280 °F |
Average value: 140 µm/m-°C Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |