Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ASTM D-696 |
Plaskolite Optix® CA - 1000 E-2 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ASTM D-696 |
Plaskolite Optix® CP - 1000 I High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CA - 1000 I High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CP - 1000 E High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359 |
PTS POM-90 Acetal Copolymer Information provided by PTS LLC. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ASTM D-696 |
Plaskolite West Optix® CA - 1000 E High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
CTE, linear | 120 - 140 µm/m-°C @Temperature 20.0 °C |
66.7 - 77.8 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
CTE, linear | 120 - 140 µm/m-°C @Temperature 20.0 °C |
66.7 - 77.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Solef® 3208/0150 Anti-friction PVDF Compound
(discontinued **) Key features of this grade: Anti-friction, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | Above Tg |
EVALCA EVAL® K102 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ASTM D696 |
Kolon SPESIN® KP213HIBL Impact Resistant PBT Compound resin Impact resistant, BLACKApplications: Wiper bladesInformation provided by API-Kolon. |
|||
CTE, linear | 120 µm/m-°C @Temperature 20.0 °C |
66.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ineos G50-100 HDPE Ineos G50-100 is a high molecular weight, high density polyethylene copolymer developed for sheet extrusion, thermoforming and large part blowmolding where the finished product demands outstanding p.. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ASTM E831 |
Lucite International Diakon® TD735 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
CTE, linear | 120 - 200 µm/m-°C | 66.7 - 111 µin/in-°F | 25°C to 100°C; ASTM D696 |
Guarniflon MFA Fluoropolymer It’s a semi-crystalline fully-fluorinated melt processable fluoropolymer which offer the highest temperature rating and broadest chemical resistance of all melt processable fluoropolymers. It .. |
|||
CTE, linear | 120 µm/m-°C @Temperature 20.0 °C |
66.7 µin/in-°F @Temperature 68.0 °F |
|
Total 3802 Blue MDPE pipe, injection molding FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth.. |
|||
CTE, linear | 120 µm/m-°C @Temperature 23.0 - 60.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 140 °F |
ASTM D696 |
Daikin NEOFLON AP-230 PFA Pellets NEOFLON PFA pellets have good melt flowability, and can be processed in the same manner as other thermoplastic resins.Applications: Linings, tubing, etc.Information provided by Daikin Industries. |
|||
CTE, linear | 120 µm/m-°C @Temperature 20.0 °C |
66.7 µin/in-°F @Temperature 68.0 °F |
DIN 53 752 |
Brandenburger BL 70 Slide Bearing Material BL 70 is a low friction material that exhibits stability at high temperatures. Its applications include high-load low friction tracks and linings in transport and conveying systems, high-stressed b.. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359 |
BLUESTAR BS130 Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ISO 11359 |
BLUESTAR BS270 Acetal Copolymer Information provided by Polymer Technology and Services, LLC (PTS). |
|||
CTE, linear | 120 - 200 µm/m-°C | 66.7 - 111 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Hyflon® PFA 120X Perfluoroalkoxy (PFA)
(discontinued **) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resis.. |
|||
CTE, linear | 120 - 130 µm/m-°C | 66.7 - 72.2 µin/in-°F | ASTM D696 |
Guarniflon PTFE G412 Polytetrafluoroethylene 15% Graphite PTFE G Standard Compound with graphite.Properties: Extremely low coefficient of friction. Fairly good compressive strength. Enhanced chemical resistance. Good wear resistance. Good thermal diss.. |
|||
CTE, linear | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® M90-45 Acetal Co-polymer (POM), Weather resistance, General DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 120 µm/m-°C | 66.7 µin/in-°F | ASTM E831 |
Lucite International Diakon® ST45G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed by in.. |
|||
CTE, linear | 120 µm/m-°C @Temperature 23.0 - 55.0 °C |
66.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® M90-44/M90S Acetal Co-polymer (POM), Standard, General DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |