Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.2 µm/m-°C @Temperature 600 °C |
6.78 µin/in-°F @Temperature 1110 °F |
|
Outokumpu 4724 High Temperature Ferritic Stainless Steel Truly stainless high temperature grade with 13% chromium. Not critical in terms of embrittlement.Applications: Mostly used in high temperature applications with sulphurous atmospheres and/or low te.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 °C |
6.78 µin/in-°F @Temperature 68.0 °F |
|
Hogen Duralloy H5TC 50 Tungsten Carbide/50 Copper PM Metal Composite Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Used for light duty projection weld.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 - 100 °C |
6.78 µin/in-°F @Temperature 68.0 - 212 °F |
|
Misumi DC53 JIS Tool Steel General purpose cold work die and mold steel whose strength and toughness approach those of high speed steels. Good machinability and grindability. Tougher than D2 Tool Steel. Machines 30% faster th.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 - 100 °C |
6.78 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals INCONEL® Alloy C-276 A nickel-molybdenum-chromium alloy with an addition of tungsten having excellent corrosion resistance in a wide range of severe environments. The high molybdenum content makes the alloy especially .. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 - 100 °C |
6.78 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals INCONEL® Alloy MA 754 A mechanically alloyed nickel-chromium alloy with oxide dispersion strengthening. Mechanical alloying, which involves high-energy milling of metal powders, is used to create a uniformly distributed.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 - 100 °C |
6.78 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals NIMONIC® Alloy 105 A precipitation-hardenable nickel-cobalt-chromium alloy with an addition of molybdenum for solid-solution strengthening. The relatively high aluminum content enhances both strength (through greater.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 °C |
6.78 µin/in-°F @Temperature 68.0 °F |
|
California Fine Wire Permanickel® K-300 Nickel Alloy All values may vary dependent on specific design and usagePermanickel® is a registered trade name of the Inco family of products.Capabilities: WireRibbonInsulatedPlatedInformation provided by Calif.. |
|||
CTE, linear | 12.2 µm/m-°C @Temperature 20.0 °C |
6.78 µin/in-°F @Temperature 68.0 °F |
|
California Fine Wire Stablohm 800 Nickel, Chromium, Aluminum, and Copper Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |