Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | Y; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9338 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | X; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NX9240 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | X; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NX9245 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | X; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NX9260 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 12.0 - 500 µm/m-°C | 6.67 - 278 µin/in-°F | Average value: 104 µm/m-°C Grade Count:15 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 °C |
6.67 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® SMT-B-1F Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for PBGA applications. It has the same unique resin system as SMT-B-1, which mi.. |
|||
CTE, linear | 12.0 - 79.2 µm/m-°C | 6.67 - 44.0 µin/in-°F | Average value: 28.1 µm/m-°C Grade Count:23 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 °C |
6.67 µin/in-°F @Temperature 68.0 °F |
|
Hoskins Manufacturing Alumel® Thermocouple Wire Type K - Std All values may vary dependent on specific design and usageAlumel® is a registered trade name of Hoskins Manufacturing.Capabilities: WireRibbonSquareInsulatedPlatedInformation provided by Californ.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 260 °C |
6.67 µin/in-°F @Temperature 500 °F |
|
Ferro EG 2783 Thick Film Glass Glass Type: Pb-B Typical Powder Form: MVG Typical Application: Die Attachment Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conduct.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 37.8 - 538 °C |
6.66 µin/in-°F @Temperature 100 - 1000 °F |
|
Meehanite HE Heat Resisting Cast Iron Type HE is a freely machinable material in the as-cast condition. Withstands rapid heating and cooling without premature failure, offers good dimensional stability and a good range of strength prop.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | ISO 11359-2 |
Menzolit Menzolit® BMC 2400 Unsaturated Polyester UP BMC 2400 is a general purpose BMC for applications in the field of low smoke density and non toxic smoke.. The flammability meets the demands of EN45545 and is classified according to British standa.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | ISO 11359-2 |
Menzolit Menzolit® SMC 0200 Unsaturated Polyester UP SMC 0200 is a general purpose SMC for a wide range of applications. Typically, it is used as housings, covers and functional components in mechanical engineering. The flammability meets the demands .. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | ISO 11359-2 |
Menzolit Menzolit® SMC 0800 Unsaturated Polyester UP SMC 0800 is a special SMC for applications within househould and kitchenware. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The product .. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | ISO 11359-2 |
Menzolit Menzolit® SMC 0900 Unsaturated Polyester UP SMC 0900 is a special SMC for use within a chemical aggressive environment. The glass level is selected to combine good mouldability with good strength and stiffness properties. The product is espec.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | ISO 11359-2 |
Menzolit Menzolit® SMC 1650 Unsaturated Polyester UP SMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in .. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | ISO 11359-2 |
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP SMC 2600 is a special SMC with electrically conductive properties. Because of its conductivity, SMC 2600 is antistatic and prevents build-up of electrical charges on the surface. Despite of its cond.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | |
Mo-Sci Corporation GAI-40-I Green A Intruder Filter Glass Applications: Lead-free NVIS Green A Intruder filter glass for incandescent light sources.Information provided by Mo-Sci Corporation. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 750 °C |
6.67 µin/in-°F @Temperature 68.0 - 1380 °F |
BSÂ 1902: section 5.3: 1990 |
Skamol Group VIP 12 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | |
Master Bond EP30LTE-LO Dimensionally Stable Low Outgassing Two Part Epoxy Master Bond Polymer System EP30LTE-LO is a thermal shock resistant epoxy resin system with low thermal expansion properties and dimensional stability for high performance bonding, sealing and castin.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 200 °C |
6.67 µin/in-°F @Temperature 68.0 - 392 °F |
Values determined by minute linear expansion tester at 5°C/min. temperature increments |
UBE UPILEX 25S (25 micron) Polyimide Film Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | x direction |
Arlon AD300A Glass, PTFE and Micro-Dispersed Ceramic Lower Loss and Improved Performance over Traditional AD Series.Information provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | x direction |
Arlon AD250 Woven Glass and PTFE Used in the RF and microwave industries, including base station antennas and BSA feed networks.Information provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | x direction |
Arlon AD320 Glass, PTFE and Micro-Dispersed Ceramic Used in the RF and microwave industries, including base station antennas and BSA feed networks.Information provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear | 12.0 - 19.0 µm/m-°C @Temperature 55.0 - 160 °C |
6.67 - 10.6 µin/in-°F @Temperature 131 - 320 °F |
Average value: 15.5 µm/m-°C Grade Count:2 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | |
Mo-Sci Corporation GA-40-I Green A Filter Glass Applications: Lead-free NVIS Green A filter glass for incandescent light sources.Information provided by Mo-Sci Corporation. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | |
Mo-Sci Corporation GA-80-N Green Filter Glass Applications: Lead-free NVIS green filter glass for Nichia White LED sources.Information provided by Mo-Sci Corporation. |
|||
CTE, linear | 12.0 - 20.0 µm/m-°C | 6.67 - 11.1 µin/in-°F | VDE 0304T1 |
Bulk Molding Compounds tetra-DUR N 4203 Bulk Molding Compound Highest dimensional stability under temp. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipat.. |