 POLYMER SEARCH

Polymer Property : CTE, linear = 111 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 111 µm/m-°C
61.7 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® H20E-8 Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H20E-8 is a two component, silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is a higher viscos..
CTE, linear 111 µm/m-°C

@Temperature 20.0 - 160 °C
61.7 µin/in-°F

@Temperature 68.0 - 320 °F
Silicone Property; ASTM E 831
Arlon CP-594CX Bulk Compound
Product Use: Electrically insulating electronic adhesive. Bonds without primer.Appearance: Gray, high viscosity gumUL94V-0: The product is designed to meet UL94V-0 flame resistance requirements but ..
CTE, linear 111 µm/m-°C

@Temperature 20.0 - 160 °C
61.7 µin/in-°F

@Temperature 68.0 - 320 °F
Silicone Property; ASTM E 831
Arlon Thermabond® 99A50X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier..
CTE, linear 111 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
61.7 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359
Ascend Performance Materials Vydyne® 47 Nylon 66, DAM
Vydyne® 47 Nylon resins are general purpose polyamide, impact modified grades. They are available in natural, black and heat stabilized for improved resistance to elevated temperatures. The heat st..
CTE, linear 111 µm/m-°C

@Temperature 20.0 - 160 °C
61.7 µin/in-°F

@Temperature 68.0 - 320 °F
Silicone Property; ASTM E 831
Arlon R37622X008 0.008" (0.203 mm) Cured Silicone Rubber with Release PET Carrier
Description: Thermabond® electrically insulating, thermally conductive, thermal interface materialDesign/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fiber..
CTE, linear 111 µm/m-°C

@Temperature 20.0 °C
61.7 µin/in-°F

@Temperature 68.0 °F
silicone property; ASTM E 831
Arlon R37806X030 Silicone Rubber/Fiberglass
Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber