Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.4 µm/m-°C @Temperature 20.0 °C |
6.33 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Gharda Chemicals GATONE™ 5330FC Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 20.0 °C |
6.33 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Gharda Chemicals GATONE™ 5630FC Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 20.0 °C |
6.33 µin/in-°F @Temperature 68.0 °F |
|
California Fine Wire Stablohm 825 Nickel Chromium Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |