Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 102 µm/m-°C @Temperature 20.0 °C |
56.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
LG Chemical LG-749 ABS, Low Gloss, High Heat Resistance Information Provided by LG Chem |
|||
CTE, linear | 102 µm/m-°C | 56.7 µin/in-°F | ASTM-D696 |
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components. |
|||
CTE, linear | 102 µm/m-°C | 56.9 µin/in-°F | ASTM C531 |
Chesterton ARC 982 100% Novolac acid resistant coating Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. A low viscosity composite that is applied by brush, squeegee, or a plural compo.. |