Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 101 µm/m-°C @Temperature -40.0 - 149 °C |
56.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Nylatron® LFG (ASTM Product Data Sheet) |
|||
CTE, linear | 101 µm/m-°C @Temperature -40.0 - 149 °C |
56.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Nylatron® LIG Oil Filled Cast 6 Nylon (ASTM Product Data Sheet) |
|||
CTE, linear | 101 µm/m-°C @Temperature -40.0 - 176 °C |
56.0 µin/in-°F @Temperature -40.0 - 349 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylac® PL75 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
CTE, linear | 101 µm/m-°C @Temperature 20.0 °C |
56.0 µin/in-°F @Temperature 68.0 °F |
|
RedEye On Demand ABS for Rapid Prototyping ABS or Acrylonitrile butadiene styrene is a true industrial thermoplastic that is impact-resistant and structurally strong. ABS parts are built with a layered manufacturing process utilizing Fused D.. |
|||
CTE, linear | 101 µm/m-°C @Temperature 20.0 °C |
56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Acrylloy 10 Acrylic Sheet Description: Acrylic SheetInformation provided by Spartech. |
|||
CTE, linear | 101 µm/m-°C @Temperature 20.0 °C |
56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Crylex High Impact Acrylic Sign Grade Sheet Description: Sign Grade SheetInformation provided by Spartech. |
|||
CTE, linear | 101 µm/m-°C @Temperature 20.0 °C |
56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Korad® SP-9071 FR/ABS Flame Retardant Sheet Description: Flame Retardant SheetKorad is a registered trademark of Polymer Extruded Products, Inc..Information provided by Spartech. |
|||
CTE, linear | 101 µm/m-°C @Temperature 20.0 °C |
56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech SP-9013 FR/ABS Flame Retardant Sheet Description: Flame Retardant SheetInformation provided by Spartech. |
|||
CTE, linear | 101 µm/m-°C @Temperature 20.0 °C |
56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Stratasys® ABS ABS is a strong, durable production-grade thermoplastic used across many industries. ABS is an ideal material for conceptual prototyping through design verification through direct digital manufactur.. |
|||
CTE, linear | 101 µm/m-°C @Temperature 20.0 °C |
56.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Covestro Baydur® GS-772 Polyurethane Solid RIM, MDI-based 2-Component Liquid System 0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
CTE, linear | 101 µm/m-°C @Temperature 20.0 °C |
56.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Covestro Prism® CM-200 Polyurethane Solid RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
CTE, linear | 101 µm/m-°C @Temperature 20.0 °C |
56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
CPC - Vycom FLAMETEC™ HALAR® 901 Opaque Ethylene Chlorotrifluoroethylene (ECTFE) Flametec™ Halar® ECTFE (Ethylene Chlorotrifluoroethylene) is an ultra-pure fluoropolymer that is a tough engineering thermoplastic with a balance of physical and chemical properties that qualify i.. |
|||
CTE, linear | 101 - 121 µm/m-°C @Temperature 20.0 °C |
56.0 - 67.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
CPC - Vycom FLAMETEC™ KYTEC® PVDF Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when e.. |
|||
CTE, linear | 101 µm/m-°C @Temperature 20.0 °C |
56.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Halar® 901 ECTFE Made from HALAR® ethylene-chlorotrifluoroethylene resin, these products are virtually unaffected by most corrosive chemicals. ECTFE products have excellent chemical and mechanical properties, impa.. |